Welcome: Shaanxi Guangke Titanium Industry Co., Ltd.

sales@gktitanium.com +86-19539017809

Titanium Heat Exchanger Tube

Heat exchanger tube in Grade 1 and Grade 2 to ASTM B338, for shell-and-tube exchangers, condensers, coolers and reboilers. OD 6 to 50.8 mm, wall 0.5…

EMAIL

Heat exchanger tube in Grade 1 and Grade 2 to ASTM B338, for shell-and-tube exchangers, condensers, coolers and reboilers. OD 6 to 50.8 mm, wall 0.5 to 3 mm, straight or U-bent to your tube sheet layout, cut to length, eddy current tested, bores cleaned and capped.

Request a Quote

Grade by service

ServiceGradeReason
Seawater coolingGrade 2Standard choice, widest availability
Thin wall, tight U-bendGrade 1Extra ductility at the bend
Hot brine, crevice riskGrade 12Mo-Ni resists crevice attack
Reducing acidGrade 7Pd-stabilised, acid service
High-purity condensateGrade 1Formability, clean bore

Grade 2 is the default: 345 MPa tensile, enough resistance to seawater and chlorides for most cooling duty, and hard enough to take rolling without cracking. Grade 1 is the same alloy with lower oxygen and more ductility, and it goes where the wall is under about 1 mm and the bend is tight. Values above are ASTM minimums; on a code-stamped exchanger the allowable stress comes from ASME SB338.

U-bend and coplanarity

The legs have to sit in one plane. A U-tube whose legs are skewed by a millimetre or two will not line up with both tube holes at the far end of the bundle, and the fitter pulls it through with a chain fall. The tube survives that. The rolled joint usually does not.

We bend to the drawing at 1.5 × OD radius or larger, hold leg lengths to ±1.5 mm, and check coplanarity on every tube before packing. Tighter radii are quoted after we check wall thinning and ovality on the outside of the bend, which is where a U-tube fails first. Grade 2 U-bends are stress relieved on request; for sour or cyclic service say so, because it adds a heat treatment step and a day.

Bore and rolling

Exchanger tube ships pickled inside and out, with no drawing lubricant left in the bore, then capped. No carbon steel touches it through cutting and packing, because one embedded iron particle becomes a pit that starts leaking in year three. Bright annealed bore is available where the process side must stay oxide-free.

For rolling, the tube end must be annealed, round and free of longitudinal marks. Wall reduction is the fabricator's number, typically 5 to 7% for titanium, but it only repeats if the OD band is tight. Tell us the expansion method and we hold the OD at the ends.

Documents

ItemDetail
Eddy currentFull length, or hydrostatic at the calculated pressure
MechanicalFlattening and flare results, bend checks on U-tube
MTCEN 10204 3.1, heat number, chemistry, mechanicals
CleanlinessBore condition and dimensional report on request

Packing and lead time

ItemDetail
Straight tubeISPM-15 crates with V-supports, capped ends
U-tubeRacked with legs at fixed pitch, bends clear of each other
Stock sizeson request
Lead timeon request
Minimum orderon request

FAQ

Grade 1 or 2 for a seawater condenser?
Grade 2 unless the wall is thin enough that bending needs more ductility. Both resist seawater; Grade 1 just forms more easily. Under 1 mm wall at a tight radius, we would quote Grade 1.

What is your U-bend tolerance?
Leg length ±1.5 mm, radius per drawing, and legs coplanar within on request. Wall thinning at the bend is checked before packing.

Tube sheet and baffles as well?
Tube sheet plate comes as Grade 2 titanium plate, the pipe side as Grade 2 titanium pipe. One order covers tube, plate and fittings, so the fabricator is not waiting on a second delivery.

Quote

Send grade, OD, wall, straight or U-bend, leg lengths, bend radius, quantity and test requirement. A tube sheet drawing prices fastest.

Send Your Requirement

Related

INQUIRY

CATEGORIES

CONTACT US

Contact: Jessie

Phone: +86-19539017809

E-mail: sales@gktitanium.com

Add: BLOCK A, HUIHANG PLAZA , HANGTUO ROAD, NATIONAL CIVIL AEROSPACE INDUSTRY BASE, Xi'an