Titanium arrives in the condition it was inspected in, or it arrives as a claim. Packing decides which. The risks being managed are surface damage, chloride staining, condensation inside the container, load shift, and paperwork that no longer matches the crate. Each one has a cheap fix.
A bar ground to h9 carries a surface and a diameter that one strap mark can ruin. A 0.05 mm (0.002 in) nick on Ø12 mm bar is a visible defect on a part that will be polished later. Titanium also carries no corrosion allowance, so damage is not absorbed by extra wall. It is rejected or reworked.
The second difference is contamination. Free iron picked up from steel strapping or dunnage becomes a corrosion site once the part sees chloride service. Chloride residue has to come off before welding or it turns into porosity and alpha case.
Unit weights in the table are crate limits, not cargo limits. A crate under 1,000 kg can be lifted by a standard forklift at the dock.
| Form | Packing | Crate limit | Risk it controls |
|---|---|---|---|
| Bar, Ø8–60 mm | Plastic sleeve over bundle, hessian wrap, strap with edge protectors, timber cradle | 1,000 kg | Bar-to-bar abrasion, strap marking |
| Ground or polished bar | Paper or tube wrap per piece, VCI film over the bundle | 800 kg | Surface nicks read as diameter defects |
| Large bar, forgings | Timber cradle, no strap over a machined OD, lifting points marked | 1,000 kg | Crush marks on sealing faces |
| Plate, 0.5–6 mm | Plywood case, paper interleaved, edges protected | 700 kg | Edge waviness and fretting |
| Plate, over 6 mm | Timber skid, paper between sheets, banded to skid | 1,500 kg | Sheet-to-sheet abrasion |
| Tube and pipe | Ends capped, bundled, plastic wrapped, desiccant in the bag | 1,000 kg | Moisture in the bore, ovality |
| Fittings, flanges | Bag and foam per piece, partitioned crate | 500 kg | Impact damage to gasket faces |
A steel container crossing a 30 °C day and a 12 °C night condenses water on the ceiling and drips it onto the cargo. A 40 ft box can shed litres over a two-week voyage. VCI film slows surface attack and desiccant absorbs the rest, but only with the film sealed. An open bag inside an unsealed crate does nothing.
For a 30-day voyage, a working starting point is 1 kg of calcium chloride desiccant per 2–3 m³ of crate volume, with the film heat-sealed; on request. Titanium needs no rust inhibitor, so the VCI film serves as a moisture and chloride barrier.
Wood is a separate compliance question. Solid-wood packaging must be heat treated and stamped to ISPM-15; plywood is processed wood and exempt. A container held at destination for a missing stamp costs two to three weeks, more than the crate itself.
Marks are not decoration. Receiving QA, the customs broker and your goods-in team reconcile them against different documents. Every crate carries the purchase order and item number, grade with UNS number, heat number per bundle, size and length, net and gross weight, crate number against total (3 of 7), handling symbols and country of origin. Neutral marking without the supplier name is available for resale under another brand. Never neutral on the heat number, which is the only link to the mill certificate.
The failure to avoid is a mark that disagrees with the paperwork. A heat number that is not on the MTC stops the goods at incoming inspection, and the fix is a photograph, not a truck.
| Container | Internal length | Practical titanium load | Watch for |
|---|---|---|---|
| 20 GP | 5.9 m (19 ft 4 in) | 18–22 t of bar | Bars over 5.8 m; road axle limits |
| 40 GP / 40 HQ | 12.0 m (39 ft 5 in) | 22–25 t of bar | Volume runs out first on plate and tube |
Bar is a weight cargo, so the plan starts at the bottom: heaviest bundles on the floor, spread fore and aft, dunnage under every point load, centre of gravity low. Bar above 5.8 m (19 ft) needs a 40 ft box, and 12 m (39 ft 4 in) bar needs the door height checked before booking. Plate and tube invert the problem. They cube out first, so crate design sets the load rather than tonnage.
The set that travels with the goods: packing list with heat numbers per bundle, mill test certificate to EN 10204 3.1, commercial invoice, certificate of origin, ISPM-15 declaration or stamp record, and safety data for any coating or VCI product. Photographs of the packed crate before the doors close settle most damage claims before they start. The documents and certificates page lists the standard set, and the packing and logistics page covers crating and ports.
Detail changes with the form. Grade 5 titanium bar travels as strapped bundles on a cradle, Grade 2 titanium plate as interleaved sheets in a plywood case, and Grade 2 heat exchanger tube capped and bagged so the bore is clean on arrival.
Send the destination port, the form and size, whether the crates have to stack, and any neutral-marking requirement. We will quote packing and freight on the same basis, with marks and documents fixed before the goods are crated.
Contact: Jessie
Phone: +86-19539017809
E-mail: sales@gktitanium.com
Add: BLOCK A, HUIHANG PLAZA , HANGTUO ROAD, NATIONAL CIVIL AEROSPACE INDUSTRY BASE, Xi'an